System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Angst+Pfister APSOplast® VESPEL PI SP1 PI
Categories:
Polymer
;
Thermoplastic
;
Polyimide, Thermoplastic
Material Notes:
PI SP1 is the unfilled standard type with maximum strength and elongation and the lowest modulus of elasticity. In addition, this material has a low thermal conductivity and optimum electrical properties.
Information provided by Angst + Pfister
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.43
g/cc
0.0517
lb/in³
DIN EN ISO 1183-1
Moisture Absorption
1.30 %
1.30 %
at saturation in standardized climate; DIN EN ISO 62
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
86.0
MPa
12500
psi
ASTM D 1708
Elongation at Break
7.5 %
7.5 %
ASTM D 1708
Modulus of Elasticity
3.10
GPa
450
ksi
ASTM D 790
3.28
GPa
476
ksi
ASTM D 638
Izod Impact, Notched
0.427
J/cm
0.800
ft-lb/in
ASTM D 256
Izod Impact, Unnotched
7.47
J/cm
14.0
ft-lb/in
ASTM D 256
Coefficient of Friction
0.35
0.35
p=0.05 N/mm2, v=0.6 m/s, against hardened and polished steel
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+14
-
1.00e+15
ohm-cm
1.00e+14
-
1.00e+15
ohm-cm
ASTM D 257
Surface Resistance
1.00e+14
-
1.00e+16
ohm
1.00e+14
-
1.00e+16
ohm
ASTM D 257
Dielectric Constant
3.62
@Frequency 100 Hz
3.62
@Frequency 100 Hz
ASTM D 150
Dielectric Strength
22.0
kV/mm
559
kV/in
ASTM D 149
Dielectric Loss Index
0.0018
@Frequency 100 Hz
0.0018
@Frequency 100 Hz
ASTM D 150
Thermal Properties
Metric
English
Comments
CTE, linear
54.0
µm/m-°C
@Temperature 23.0 - 60.0 °C
30.0
µin/in-°F
@Temperature 73.4 - 140 °F
Specific Heat Capacity
1.13
J/g-°C
0.270
BTU/lb-°F
Thermal Conductivity
0.350
W/m-K
2.43
BTU-in/hr-ft²-°F
Maximum Service Temperature, Air
300
°C
572
°F
long term
360
°C
680
°F
short term
Deflection Temperature at 1.8 MPa (264 psi)
360
°C
680
°F
DIN EN ISO 75 / A
Flammability, UL94
V-0
V-0
Descriptive Properties
Color
brown
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PANGP070 / 250568
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.