MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Cabot CAB-O-SILĀ® MS-75D Fumed Silica
Categories: Other Engineering Material

Material Notes: Product highlights: CAB-O-SIL MS-75D fumed silica, the densed form of CAB-O-SIL MS-55 fumed silica, is a medium-high surface area fumed silica that reinforces silicone rubber. The higher bulk density of CAB-O-SIL MS-75D fumed silica allows for faster incorporation and easier handling. All untreated fumed silicas are characterized by:
  • High purity
  • Aggregated structure
  • Submicron particle size
  • Low bulk density
  • Hydrophilic surface chemistry
Key applications: CAB-O-SIL MS-75D fumed silica is suitable for use in the reinforcement of silicone rubbers, including heat-cured rubber, high temp vulcanizing or high consistency rubber (HTV or HCR) and liquid silicone rubber (LSR), in which it can increase hardness, tensile strength and elongation. Due to the hydrophilic surface of CAB-O-SIL MS-75D fumed silica, further modification of its surface is necessary to prevent crepe hardening. With use of a densed, higher bulk density silica, such as CAB-O-SIL MS-75D fumed silica, the use of very high shear dispersion equipment is recommended to achieve adequate dispersion of the silica. The higher bulk density of this product facilitates faster wet-in or incorporation into viscous polymer systems.

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Product FormPowder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCABOT091 / 315826

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.