MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Akrochem PROAID® AC 18E Process Aids
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: PROAID AC 18E is an unsaturated erucamide primarily used as a surface lubricant in rubber articles and as an antiblock/slip agent in polyolefin films (LDPE and PP). In rubber it will bloom at low loadings (1-2 phr in NBR and CR; 3-5 phr in EPDM) from most elastomers creating a low coefficient of friction on the surface of molded goods. Proaid AC 18E will provide a non-oily, non-greasy lubricating film on exposed rubber surfaces. AC 18E is slowest out of EPDM (allow 72 hrs for bloom to form in EPDM). This material also acts as a process aid in all polymers, particularly as a mold release aid.

Applications: Proaid AC 18E’s surface lubrication effect can be used to improve a rubber's resistance to sliding abrasion, prevent galling of parts to dry metal surfaces, ease installation of rubber parts by letting them "slip" into position, and reduce sticking together of cured parts. Suggested Loadings: 0.25 - 2.00 phr for reduced surface tack on cured parts. 3.00 - 5.00 phr for low coefficient of friction surface and improved abrasion wear. Add up to 10 phr for a longlasting bloom that is self-restoring. Due to the unsaturation in the erucamide, Proaid AC 18E may possibly have a greater reduction effect on the rubber’s state-of-cure than Proaid LCF (our other low coefficient-of-friction additive). AC 18E will bloom clearer than Akrochem’s Proaid LCF. Proaid AC 18E has FDA listing in CFR 21 Sections 175.105, 175.300, 176.180, 177.1200, 177.1210, 177.1350, 177.1400, and 178.3860.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.870 g/cc0.870 g/cc
 
Chemical PropertiesMetricEnglishComments
Acid Value 0.500.50
 
Thermal PropertiesMetricEnglishComments
Melting Point 80.0 °C176 °F
 
Optical PropertiesMetricEnglishComments
Gardner Color Number 1.01.0
 
Descriptive Properties
Appearancefree flowing white beads
Iodine Value77

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH362 / 315280

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.