SABIC LNP™ LUBRICOMP™ Compound RA004 Polyamide 66 (Nylon 66)
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
Material Notes:
LNP LUBRICOMP RA004 compound is based on Nylon 6/6 resin containing 20% aramid fiber. Added features of this grade include: Wear Resistant.
Features: Wear resistant
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.20
g/cc
0.0434
lb/in³
ISO 1183
1.23
g/cc
0.0444
lb/in³
ASTM D792
Moisture Absorption
0.150 - 0.250 %
0.150 - 0.250 %
Injection Molding
Linear Mold Shrinkage, Flow
0.015
cm/cm
0.015
in/in
24hrs; ASTM D955
Linear Mold Shrinkage, Transverse
0.020
cm/cm
0.020
in/in
24hrs; ASTM D955
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
85.0
MPa
12300
psi
5 mm/min; ISO 527
88.0
MPa
12800
psi
ASTM D638
Elongation at Break
3.6 %
3.6 %
5 mm/min; ISO 527
4.5 %
4.5 %
ASTM D638
Flexural Strength
122
MPa
17700
psi
break, 2mm/min; ISO 178
137
MPa
19900
psi
ASTM D790
Flexural Modulus
4.00
GPa
580
ksi
2 mm/min; ISO 178
4.41
GPa
640
ksi
ASTM D790
Izod Impact Notched
32.0
J
23.6
ft-lb
ASTM D256
Izod Impact, Unnotched
3.68
J/cm
6.89
ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO)
5.00
kJ/m²
2.38
ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO)
40.0
kJ/m²
19.0
ft-lb/in²
80*10*4; ISO 180/1U
Coefficient of Friction, Dynamic
0.52
0.52
ASTM D3702 Modified: Manual
Coefficient of Friction, Static
0.66
0.66
ASTM D3702 Modified: Manual
K (wear) Factor
119
x 10
-8
mm³/N-M
59.0
x 10
-10
in³-min/ft-lb-hr
Washer; ASTM D3702 Modified: Manual
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
60.0
µm/m-°C
@Temperature 23.0 - 60.0 °C
33.3
µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow
90.0
µm/m-°C
@Temperature 23.0 - 60.0 °C
50.0
µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi)
199
°C
390
°F
Flatw 80*10*4 sp=64mm; ISO 75/Af
171
°C
@Thickness 3.20 mm
340
°F
@Thickness 0.126 in
unannealed; ASTM D648
Processing Properties
Metric
English
Comments
Zone 2
280
-
295
°C
536
-
563
°F
Zone 3
295
-
305
°C
563
-
581
°F
Melt Temperature
275
-
290
°C
527
-
554
°F
Injection Molding
Mold Temperature
80.0
-
95.0
°C
176
-
203
°F
Drying Temperature
80.0
°C
176
°F
Injection Molding
Dry Time
4.00
hour
4.00
hour
Injection Molding
Back Pressure
0.200
-
0.300
MPa
29.0
-
43.5
psi
Screw Speed
30
-
60
rpm
30
-
60
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PSABH80955 / 288902
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.