MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Indium Corp. IndiTri™ InCl3-4H2O Indium Trichloride Hydrate
Categories: Ceramic; Halide

Material Notes: Indium Trichloride is a white, odorless and highly deliquescent powder. Its particles are flake shaped and highly soluble in water and mineral acids. It is used as a starting chemical for the synthesis of other inorganic indium compounds and as an additive to alkaline batteries to reduce outgassing and improve electrical load. Indium Trichloride is available as an anhydrous powder and as a solution up to its solubility limit.
  • White deliquescent powder
  • Uses: Chemical synthesis; alkaline battery additive
  • Purity Grades Available: 4N (99.99%), 5N (99.999%)
  • Crystalline Form: White plates, deliquescent
  • Isomorphous with: AlCl3, YCl3
  • Coordination Number: 6

Information Provided by Indium Corporation

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.97 g/cc1.97 g/ccSaturated Solution
 3.46 g/cc3.46 g/ccSolid, Anhydrous
Solubility in Water 66.11 %
@Temperature 22.0 °C
66.11 %
@Temperature 71.6 °F
Solid, Anhydrous
Molecular Weight 293.18 g/mol293.18 g/molHydrate
 
Thermal PropertiesMetricEnglishComments
Melting Point 586 °C1090 °FSolid, Anhydrous
Boiling Point 600 °C1110 °FVolatizes (Solid, Anhydrous)
Sublimation Temperature 300 °C572 °FSolid, Anhydrous
 
Component Elements PropertiesMetricEnglishComments
Indium, In 39.16 %39.16 %Theoretical, Hydrate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NNIN943c / 249289

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.