MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Cabot CAB-O-SILĀ® EH-5 Fumed Silica
Categories: Other Engineering Material

Material Notes: CAB-O-SIL EH-5 fumed silica is a very high surface fumed silica which can increase the viscosity of liquid systems and provide significant reinforcement of silicone and organic rubbers.

All untreated fumed silicas are characterized by:

  • High purity
  • Aggregated structure
  • Submicron particle size
  • Low bulk density
  • Hydrophilic surface chemistry
Application Information:
Rheology Control for Coatings, Adhesive and other Liquid Systems: CAB-O-SIL EH-5 fumed silica can be used to provide thickening, thixotropic (shearthinning), and anti-settling behavior in liquid systems. Very high shear dispersion equipment is required to realize the full benefits of this product. For clear coatings and other systems, very well dispersed CAB-O-SIL EH-5 fumed silica provides greater transparency than lower surface area fumed silicas. Untreated fumed silicas are most efficient in non-polar to medium polar systems for building viscosity and improving sag-resistance. For more polar systems, treated fumed silicas may be more efficient.
Reinforcement of Silicone and Organic Rubber: CAB-O-SIL EH-5 fumed silica can be used for reinforcement of silicone rubber and can be used to reinforce organic rubbers. It imparts good increase in hardness, tensile and elongation. For clear silicone rubber applications, well-dispersed CABO-SIL EH-5 fumed silica provides excellent transparency.

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCABOT075 / 315810

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.