Accomplished with well electric ability & chemical resistance; Well ability of lubrication to act as plastic lubrication Advantages: - GOYENCHEM-CH6A provide excellent flow properties
- Accomplished with well electric ability & chemical resistance
- Well ability of lubrication to act as plastic lubrication
- Can enhance the flow properties of Polyethylene, polypropylene, ABS; the property of mold release of polymethyl methacrylate, polycarbonate while acting as the release agent
- Perfect light fastness toward TGIC polyester powder coatings
- Can be applied as the adjustment of melt flow rates
- Using GOYENCHEM-CH6A in the painting such as
- Polyester resin / epoxy resin / matting curing agent can
- improve its ability of impact resistant and softening
- GOYENCHEM-CH6A can reduce the smoothness of the surface and anti-scratches
- Improve the brightness and processing lubrication toward PVC pipes and profiled materials film and other rubbery item
- Can be applied as dispersion and lubricant agent toward plastic master etch and pigment
- Processing modification agent of plastic and elastomers, inks and paper coating slurry polishing agent
Applications: - Polyethylene / polypropylene / ABS
- Poly (methyl methacrylate) / polycarbonate
- TGIC powder coating curing polyester
- Polyester resin / epoxy resin / matting curing agent
- PVC pipes profile film and other plastics and rubber processing products
- Plastic master batch lubricant and dispersant
- The plastic and elastomeric processing modifier
- Ink paste polishes
- Paper coating
- Candles
Information provided by Go Yen Chemical |