MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubrizol Advanced Materials Estane® 2355-95AEF TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Product Description: This product is a thermoplastic polyurethane elastomer; Features: Film resin, Fuel resistant, Blown molding grade resin

Availability: Latin America; North America

Features: Fuel Resistant

Uses: Blow Molding Applications; Film

Form: Pellets

Processing Method: Blow Molding

Information provided by Lubrizol Advanced Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0090 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.0060 - 0.0090 cm/cmASTM D955
Melt Flow 13 g/10 min
@Load 8.70 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 94ASTM D2240
Tensile Strength at Break 5640 psiASTM D412
Tensile Stress 1200 psi
@Strain 50 %,
Thickness 3.20 mm
ASTM D412
 1410 psi
@Strain 100 %,
Thickness 3.20 mm
ASTM D412
 3100 psi
@Strain 300 %,
Thickness 3.20 mm
ASTM D412
Elongation at Break 60 %
@Thickness 3.20 mm
Set After Break; ASTM D412
 450 %
@Thickness 3.20 mm
ASTM D412
Tear Strength 600 pli
@Thickness 3.20 mm
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 4.0H-22 Wheels; ASTM D1044
Compression Set 30 %
@Temperature 25.0 °C,
Time 79200 sec
ASTM D395B
 80 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395B
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Transverse to Flow 85.0 µin/in-°FASTM D696
 
Processing PropertiesOriginal ValueComments
Melt Temperature 360 - 390 °FExtrusion
Mold Temperature 61.0 - 140 °FInjection
Drying Temperature 190 - 219 °FInjection
 190 - 219 °FExtrusion
Dew Point <= -40.0 °FInjection
 <= -40.0 °FExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLUBRZ785 / 311478

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.