MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Plastcom SLOVALEN PC 93 T 10 Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Mineral Reinforced

Material Notes: Modified PP copolymer for injection molding with the content of 10% mineral filler, UV stabilized.

Application in automotive interior industry. Very good scratch and odor resistant. Delivered in natural and in the full RAL color scale.

Application: Injection molding.

Information Provided by Plastcom spol. s r.o.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.970 g/cc0.0350 lb/in³STN EN ISO 1183-1
Linear Mold Shrinkage, Flow 0.0090 cm/cm0.0090 in/inSTN EN ISO 294-4
Linear Mold Shrinkage, Transverse 0.013 cm/cm0.013 in/inSTN EN ISO 294-4
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 235 °C
20 g/10 min
@Load 4.76 lb,
Temperature 455 °F
STN EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 22.0 MPa3190 psiSTN EN ISO 527-2
Elongation at Break 5.0 %5.0 %STN EN ISO 527-2
Tensile Modulus 1.60 GPa232 ksiSTN EN ISO 527-2
Flexural Strength 24.0 MPa3480 psiSTN EN ISO 178
Flexural Modulus 0.900 GPa131 ksiSTN EN ISO 178
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
STN EN ISO 179
 NB
@Temperature -20.0 °C
NB
@Temperature -4.00 °F
STN EN ISO 179
Charpy Impact, Notched  0.400 J/cm²
@Temperature -20.0 °C
1.90 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
STN EN ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 150 °C302 °FDSC; STN EN ISO 11357-1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 250 °C392 - 482 °F
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °F
Drying Temperature 80.0 °C
@Time 14400 sec
176 °F
@Time 4.00 hour
Injection Pressure 70.0 - 90.0 MPa10200 - 13100 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPLACN935 / 282527

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.