MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Covestro Desmopan® 3385A Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Extrusion- and injection molding grade; good wear resistance; short cycle times; high melt stability; Application; hard - soft systems; Hoses, non-reinforced; Profiles; Injection molded engineering parts

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85ISO 868
Hardness, Shore D 33ISO 868
Tensile Strength, Ultimate 52.0 MPa200 mm/min; DIN 53504
Tensile Stress at Strain 2.00 MPa
@Strain 10 %
200 mm/min; DIN 53504
 4.70 MPa
@Strain 50 %
200 mm/min; DIN 53504
 5.80 MPa
@Strain 100 %
200 mm/min; DIN 53504
 16.6 MPa
@Strain 300 %
200 mm/min; DIN 53504
Elongation at Break 531 %200 mm/min; DIN 53504
Tensile Modulus 0.0210 GPa
@Temperature 60.0 °C
storage; ISO 6721-1,-4
 0.0280 GPa
@Temperature 20.0 °C
storage; ISO 6721-1,-4
 0.0840 GPa
@Temperature -20.0 °C
storage; ISO 6721-1,-4
Rebound 50 %Resilience; ISO 4662
Tear Strength 70.0 kN/m500 mm/min; ISO 34-1
Abrasion 25mm³, Method A; ISO 4649
Compression Set 15 %
@Temperature 23.0 °C
72 hr; ISO 815
 42 %
@Temperature 70.0 °C
24 hr; ISO 815
 
Processing PropertiesOriginal ValueComments
Melt Temperature 175 - 205 °CExtrusion
 190 - 210 °CInjection
Mold Temperature 20.0 °CInjection
Drying Temperature 80.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Desmopan® 3485A Polyurethane
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
Covestro Desmopan® 385 E Polyurethane
Covestro Desmopan® 9380A Thermoplastic Polyurethane
Covestro Desmopan® 385 S Polyurethane

PB09756 / 92596

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.