MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

BigRep TPU Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyurethane, TP

Material Notes: BigRep TPU has been expertly developed and tested for use with BigRep’s largest industrial 3D printers, the BigRep ONE and STUDIO, on the standard extruders with 1 mm and 0.6 mm nozzles

TPU AT A GLANCE:

  • Flexible (Shore 98 A)
  • Temperature resistance up to 100°C
  • Very high-impact strength
  • UV resistant
  • Durable, with excellent damping behavior
  • Dynamic properties
  • Chemical resistant (for wide range of chemicals)

Information provided by Bigrep

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³
Filament Diameter 2850 µm2850 µm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 40.0 MPa5800 psiISO 527
Elongation, Ultimate 470 %470 %ISO 527
Tear Strength 175 kN/m999 pliISO 34-1B
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 115 °C239 °FISO 306
 
Descriptive Properties
Filament Net Weight2.0 Kg
Heating Bed0-60°C
Print Temperature Guideline195-230°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBIGR004 / 250854

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.