Description: K-710e and K-710p are expandable polystyrene grades containing pentane as a blowing agent. The products are delivered in the form of spherical beads with a bulk density of about 0.6 g/cm3. K-710e is available in 1050 kg octabins and K-710p in 1100 kg octabins. Applications: The properties of K-710e/p make it suitable for the production of thick-walled shape-moulded products as well as heavy insulation board by block moulding. Information provided by BEWi Synbra |