Ultraform N 2320 U035 LEV AT is a UV stabilized, rapidly freezing general-purpose injection molding POM grade designed to achieve low emission and smell. Applications: Typical applications include gas filler caps, irrigation systems, windshield wiper clips and loud speaker grills. Information provided by BASF. |