Alcosperse 787 is a novel hydrophobically modified acrylic copolymer dispersing agent developed to help formulators create innovative waterborne paints and coatings with excellent performance characteristics over competitive dispersants such as water mark resistance, alkaline and salt resistance, and other related hydrotropic effects.Information provided by Nouryon |