MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Formosa Plastics Formolene® FR2375C LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: Product Description: Formolene® FR2375C is a low density polyethylene with films exhibiting good stiffness and optical properties. Formolene® FR2375C is formulated without slip and antiblock for use in film applications offering excellent extrusion processing and very good balance of mechanical and optical properties. Formolene® FR2375C meets all requirements of the US FDA as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact.

Availability: North America

Features: Excellent Processability; Food Contact Acceptable; Good Optical Properties; Good Stiffness; Low Density

Uses: Agricultural Applications; Blending; Film; Laminates; Shrink Wrap

Agency Ratings: FDA 21 CFR 177.1520

Form: Pellets

Processing Method: Coextrusion; Extrusion; Film Extrusion

Information provided by Formosa Plastic Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.923 g/ccASTM D1505
Melt Flow 0.75 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 310 %
@Thickness 0.0508 mm
Blown Film; ASTM D882
Film Elongation at Break, TD 530 %
@Thickness 0.0508 mm
Blown Film; ASTM D882
1% Secant Modulus 35000 psi
@Thickness 0.0508 mm
MD, Blown Film; ASTM D882
 40000 psi
@Thickness 0.0508 mm
TD, Blown Film; ASTM D882
Elmendorf Tear Strength MD 350 g
@Thickness 0.0508 mm
Blown Film; ASTM D1922
Elmendorf Tear Strength TD 150 g
@Thickness 0.0508 mm
Blown Film; ASTM D1922
Dart Drop Test 180 g
@Thickness 0.0508 mm
Blown Film; ASTM D1709
Film Tensile Strength at Break, MD 4000 psi
@Thickness 0.0508 mm
Blown Film; ASTM D882
Film Tensile Strength at Break, TD 3200 psi
@Thickness 0.0508 mm
Blown Film; ASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 8.4 %
@Thickness 0.0432 mm
Blown Film; ASTM D1003
Gloss 59 %
@Thickness 0.0500 mm
45°, Blown Film; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 356 - 374 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PFPCR755 / 311448

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.