MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Premix Thermoplastics PRE-ELEC® CP 1316  (discontinued **)
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: PRE-ELEC CP 1316 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resistivity PRE-ELEC CP 1316 has good mechanical properties and is easy to extrude or injection mould.

Typical applications include flexible extruded profiles and tubes and flexible injection molded parts. PRE-ELEC CP 1316 may also be used as a masterbatch and blended with EVA or PE-LD.

Test Specimen - 4.0 mm thick, 10.0 mm wide molded rod.

Information provided by Premix Thermoplastics Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 g/cc
Linear Mold Shrinkage 0.012 cm/cmISO 294-4
Melt Flow 0.040 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 0.20 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 93ISO 868
Hardness, Shore D 43ISO 868
Tensile Strength, Ultimate 11.0 MPaISO 527
Elongation at Break 500 %ISO 527
Modulus of Elasticity 0.110 GPaISO 178
Izod Impact, Notched NB
@Thickness 4.00 mm,
Temperature 23.0 °C
ISO 180
Izod Impact, Unnotched NB
@Thickness 4.00 mm,
Temperature 23.0 °C
ISO 180
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 100 ohm-cmISO D-257
Surface Resistance <= 1000 ohmISO D-257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 35.0 °CISO 75/Method Bf
Vicat Softening Point 50.0 °CRate A; ISO 306/A50
 
Processing PropertiesOriginal ValueComments
Middle Barrel Temperature 180 °CZone 1; Cylinder
 180 °CZone 2; Cylinder
 190 °CZone 3; Cylinder
 190 °CZone 4; Cylinder
 200 °CZone 5; Cylinder
 200 °CZone 6; Cylinder
Die Temperature 374 °FZone 3
 392 °FZone 4
 392 °FZone 1
 392 °FZone 2
 392 °FZone 5
Melt Temperature 180 - 220 °C
Mold Temperature 40.0 - 60.0 °C
Roll Temperature 50.0 °C3rd Roll
 60.0 °C2nd Roll
 70.0 °C1st Roll
Drying Temperature 60.0 °C
@Time >=10800 sec
If stored for longer than 1 year
Moisture Content <= 0.15 %When Produced
Injection Pressure 8702 psi
Shelf Life 12.0 MonthNormal Storing Conditions
 
Descriptive Properties
AppearanceGranule
ColorBlack
Injection SpeedModerate

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPREMA007 / 58020

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.