MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Wolf Kunststoff Zedex® ZX-324V1HT 079 PEEK
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes:

Information provided by Wolf Kunststoff

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.34 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 85.0 MPaDIN EN ISO 527
Tensile Strength 85.0 MPaDIN EN ISO 527
Tensile Strength, Yield 54.0 MPaElastic limit
Elongation at Break 4.3 %maximum force; DIN EN ISO 527
 4.3 %DIN EN ISO 527
Elongation at Yield 2.1 %Elastic yield point
Tensile Modulus 4000 MPaDIN EN ISO 527
Flexural Modulus 5000 MPaDIN EN ISO 178
K Factor (ISO) 4.5 µm/km
@Temperature 200 °C
 4.6 µm/km
@Temperature 20.0 °C
 8.7 µm/km
@Temperature 100 °C
Charpy Impact, Notched NBEN ISO 179/1eA
Coefficient of Friction, Dynamic 0.18
@Temperature 20.0 °C
 0.18
@Temperature 100 °C
Coefficient of Friction, Static 0.38
@Temperature 20.0 °C
Limiting Pressure Velocity 0.0667 MPa-m/secv=1m/min
 1.2667 MPa-m/secv=10m/min
 
Electrical PropertiesOriginal ValueComments
Dissipation Factor 0.14
@Frequency 1 Hz
tangent
 
Thermal PropertiesOriginal ValueComments
CTE, linear 40.0 µm/m-°C
@Temperature 100 °C
ISO E 830
 42.0 µm/m-°C
@Temperature 150 °C
ISO E 831
Melting Point 340 °C
Maximum Service Temperature, Air 150 °Cfor bushings when pressed
 240 °Clong term; UL 746B
 260 °C3 h
Deflection Temperature at 1.8 MPa (264 psi) 185 °CDIN EN ISO 75
Glass Transition Temp, Tg 160 °C
 
Descriptive Properties
ColorBeige
Injection molded partsApplicable
Machined partsApplicable
Plastic granulesApplicable
Rods up to øe (de)Applicable
Sheets up to max. thicknessApplicable
Tubes (hollow rods) up to øe (de)Applicable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PZEDEX3000 / 250057

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.