MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Inov Chem DLQ-A/B Air Filter Foam System
Categories: Polymer

Material Notes: Applications: It is widely used for manufacturing cars, ships, construction machinery, generator set and other internal combustion machinery's air filter cores etc.

Characteristics: A component of Polyurethane systems of air filter (DLQ-A)is composed of hyperactive polyether polyols, cross linking agent, compound catalyst and so on. B component (DLQ-B)is modified isocyanate, and it is micro-pore elastomer which adopts cold molding. It has excellent mechanical and anti-fatigue property. Also, with short production cycle, high efficiency and low energy consumption.

Information provided by Shandong INOV Polyurethane Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.300 - 0.400 g/ccOverall Density
 
Processing PropertiesOriginal ValueComments
Mold Temperature 40.0 - 45.0 °C
 
Descriptive Properties
Demolding Time7-10 min
Ratio100/30-100/40Polyol/Iso

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PINOVCHM213 / 312742

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.