19-103-000-009 Natural 19-103-000-010 BlackDescription: 33% glass fiber reinforced improved flow, heat stabilized nylon 6. Features: - Natural and black colors
- Good stiffness
- High toughness
- Low mold shrinkage
- Electrically insulating
Applications: - Electronics
- Appliances
- Automotive
Special Instructions: Minimize back pressure to maintain glass fiber integrityInformation provided by Orion Performance Compounds, Inc. |