MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Duratherm HTO22-FG Heat Transfer Fluid
Categories: Fluid

Material Notes: Duratherm HTO22-FG is ideal for a wide range of closed to atmosphere (inertly sealed) applications including food processing, paint, rubber, calendars, board plants, roofing, textiles, laundry, refineries and asphalt storage/production. Duratherm HTO22-FG is rated to 315ºC (600ºF) and engineered with a low pour point for easy starting of systems in colder climates. Duratherm HTO22-FG meets USDA requirements for incidental food contact (H1) and meets the requirements of 21CFR1783570 and is NSF registered. Duratherm HTO22-FG ensures excellent thermal stability. Its low volatility also minimizes vapor pressure at elevated temperatures and Duratherm HTO22-FG contains antioxidants, metal deactivators and corrosion inhibitors to further enhance the fluid’s longevity. Duratherm HTO22-FG is environmentally friendly, non-toxic, non-hazardous and non-reportable. Duratherm HTO22-FG poses no ill effect to worker safety. Duratherm HTO22-FG can easily be disposed of with other waste oils.

Information provided by Duratherm.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 41.4 lb/ft³
@Temperature 316 °C
ASTM D1298
 41.5 lb/ft³
@Temperature 315 °C
 43.6 lb/ft³
@Temperature 260 °C
ASTM D1298
 44.8 lb/ft³
@Temperature 230 °C
 52.3 lb/ft³
@Temperature 38.0 °C
ASTM D1298
 55.0 lb/ft³
@Temperature -30.0 °C
Viscosity 0.30 cP
@Temperature 315 °C
Dynamic
 0.68 cP
@Temperature 230 °C
Dynamic
 1915.92 cP
@Temperature -30.0 °C
Dynamic
Kinematic Viscosity 0.45 cSt
@Temperature 316 °C
ASTM D445
 0.94 cSt
@Temperature 230 °C
 5.45 cSt
@Temperature 100 °C
ASTM D445
 20.06 cSt
@Temperature 40.0 °C
ASTM D445
 2175.15 cSt
@Temperature -30.0 °C
Molecular Weight 364 g/molAverage
Vapor Pressure 0.000 atm
@Temperature 38.0 °C
ASTM D2879
 0.000 atm
@Temperature -30.0 °C
 0.0560 atm
@Temperature 260 °C
ASTM D2879
 0.220 atm
@Temperature 316 °C
ASTM D2879
 2.27 atm
@Temperature 230 °C
 22.26 atm
@Temperature 315 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 1016 µm/m-°C
Specific Heat Capacity 1.625 J/g-°C
@Temperature -30.0 °C
 1.938 J/g-°C
@Temperature 38.0 °C
 2.821 J/g-°C
@Temperature 230 °C
 2.96 J/g-°C
@Temperature 260 °C
 3.212 J/g-°C
@Temperature 315 °C
 3.215 J/g-°C
@Temperature 316 °C
Thermal Conductivity 0.103 W/m-K
@Temperature 315 °C
 0.104 W/m-K
@Temperature 316 °C
 0.107 W/m-K
@Temperature 260 °C
 0.111 W/m-K
@Temperature 230 °C
 0.128 W/m-K
@Temperature 38.0 °C
 0.133 W/m-K
@Temperature -30.0 °C
Distillation Temperature 344 - 527 °C10% to 90% range; ASTM D2887
Maximum Service Temperature, Air 315 °CBulk/Use Temp.
 343 °CFilm Temp.
Pour Point -42.0 °CASTM D97
Flash Point 186 °CASTM D93
 213 °CASTM D92
Ignition Temperature 355 °CASTM E-659-78
 
Descriptive Properties
AppearanceClear and bright liquid
Fire Point (°C)255ASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WDURA676 / 287874

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.