MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Caplinq LINQTAPE™ PIT2A-WL 2 mil white thermal ink printable polyimide film with acrylic adhesive and release liner
Categories: Polymer; Adhesive; Thermoset; Polyimide, TS; Polyimide, Thermoset Film

Material Notes: LINQTAPE™ PIT2A-WL Series is a high-temperature resistant polyimide film topped with a white, thermal-ink printable surface on one side and a permanent, acrylic-based, pressure sensitive adhesive on the backside. PIT2A-WL-Series tapes are mounted on paper release liner for easy application. LINQTAPE™PIT2A-WL-Series is designed for thermal transfer printing to create extremely durable asset tags, bar codes and bar code tags or any other alpha numeric identification labels that require extreme durability. LINQTAPE™ PIT2A-WL Series is available in Glossy and Semi-Glossy top coat layers to meet specific printing needs and preferences.

Applications:

  • Printed circuit board tracking
  • Cold/Freezer Storage
  • Extremely durable barcode and alphanumeric labels
  • Labels and tags for product identification
  • Laboratory samples
  • Outdoor applications

Information provided by Caplinq

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 22.9 microns0.900 milThermalTransfer Layer
 30.5 microns1.20 milAdhesive
 50.8 microns2.00 milFilm(Backing)
 66.0 microns2.60 milTotal
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 165 MPa24000 psi
Elongation at Break >= 55 %>= 55 %
Peel Strength 0.280 kN/m1.60 plito steel
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength >= 433 kV/mm>= 11000 kV/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Inert 260 °C500 °F
 
Descriptive Properties
Adhesion TypeAcrylic
ColorWhite
Insulation Class155 (F)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCAPL1004 / 256004

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.