MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Persian Gulf Polymer ABS-75 SW ABS Polymer
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: General purpose, Sheet, Extrusion grade. DRYING: It is recommended that ABS Resins be dried at (80-85°c) for 3 hours. Extruder with one-stage or two-stage venting are recommended for extrusion of sheet compression. Features: Sheet Grade, Extrusion grade, High rigidity& high impact strength. Typical Applications: Refrigerator interior container and door liner (cyclopentane Blowing agent use) and etc.

Information provided by Persian Gulf Polymer - Pooya Tejarat Novin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccD792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inD955
Melt Flow 4.0 - 10 g/10 min
@Load 10.0 kg,
Temperature 200 °C
4.0 - 10 g/10 min
@Load 22.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 95 - 11095 - 110D785
Tensile Strength >= 43.1 MPa>= 6250 psi50 mm/min; D638
Elongation at Break >= 25 %>= 25 %50 mm/min; D638
Flexural Strength >= 62.8 MPa>= 9110 psi2.8mm/min; D790
Flexural Modulus 1.961 GPa284.4 ksi2.8mm/min; D790
Izod Impact, Notched (ISO) >= 33.0 kJ/m²
@Thickness 6.40 mm
>= 15.7 ft-lb/in²
@Thickness 0.252 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C185 °FD648
Vicat Softening Point >= 94.0 °C
@Load 5.00 kg
>= 201 °F
@Load 11.0 lb
50°C/h; D1525
Flammability, UL94 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPERSI927 / 250331

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.