MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Vydyne® R633H Nylon 66/6, 33% Glass Reinforced, Conditioned  (Unverified Data**)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 30% Glass Fiber Reinforced

Material Notes: Vydyne® R633H is 33% glass-fiber reinforced PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold release. Vydyne R633H has tensile strength and modulus properties just below aluminum and zinc and can replace these metals in numerous applications due to an excellent balance of properties. Reduction in production costs, energy consumption, and part weight are key advantages of Vydyne glass-reinforced PA66/6 resins over aluminum and/or zinc die cast parts. Vydyne R633H is specially formulated to minimize the oxidative and thermal degradation of the PA666/6 copolymer when exposed to elevated temperatures for extended periods of time. Product provides improved retention of physical properties under exposure to long term heat. Vydyne R633H provides a higher heat distortion temperature, better resistance to creep, higher impact and better dimensional stability compared with unreinforced PA66/6. This product also provides a combination of excellent surface appearance with high tensile and modulus properties. This property balance enables usage of Vydyne R633H in applications where aesthetics and performance are important. Typical Applications/End Uses: Vydyne R633H resin has been used for many under-the-hood automotive applications, motor housings for power tools, and garden appliances. These resins have also been used in miscellaneous brackets, gears and clips that require high rigidity and strength.

Availability:

  • Asia Pacific
  • Europe
  • North America
Filler/Reinforcement:
  • Glass Fiber, 33% Filler by Weight
Additive:
  • Lubricant
  • Heat Stabilizer
Features:
  • Copolymer
  • Good Mold Release
  • Good Surface Finish
  • Heat Stabilized
  • High Tensile Strength
  • Lubricated
Uses:
  • Automotive Under the Hood
  • Gears
  • Housings
  • Lawn and Garden Equipment
  • Metal Replacement
  • Power/Other Tools
Appearance: Natural Color

Forms: Pellets

Processing Method: Injection Molding

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.39 g/ccISO 1183
Water Absorption 1.3 %
@Time 86400 sec
ISO 62
Moisture Absorption at Equilibrium 2.3 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm
@Diameter 2.00 mm
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
@Diameter 2.00 mm
ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 130 MPaISO 527-2
Elongation at Break 6.0 %ISO 527-2
Tensile Modulus 8000 MPaISO 527-2
Flexural Strength 195 MPaISO 178
Flexural Modulus 6800 MPaISO 178
Izod Impact, Notched (ISO) 19.0 kJ/m²
@Temperature -30.0 °C
ISO 180
 22.0 kJ/m²
@Temperature 23.0 °C
ISO 180
Charpy Impact Unnotched 91.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 92.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 15.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 25.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Akulon® K224-G6U PA6-GF33, Dry, 33% Glass Filled
Envalior Akulon® K224-G6U PA6-GF33, Conditioned, 33% Glass Filled

PVYDYM865 / 177216

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.