System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
SABIC LNP™ STAT-LOY™ Compound A3000XXP Acrylonitrile Butadiene Styrene (ABS)
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
Material Notes:
LNP STAT-LOY A3000XXP compound is based on Acrylonitrile Butadiene Styrene (ABS) resin containing proprietary fillers. Added features of this grade include: Permanently Anti-Static.
Features: Antistatic
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.08
g/cc
0.0390
lb/in³
ISO 1183
Moisture Absorption
0.0500 - 0.100 %
0.0500 - 0.100 %
Injection Molding
0.200 %
0.200 %
23°C/50% RH/24 hrs; ISO 62-4
Moisture Absorption at Equilibrium
0.50 %
0.50 %
23°C/50% RH; ISO 62-4
Linear Mold Shrinkage, Flow
0.0050
-
0.0070
cm/cm
0.0050
-
0.0070
in/in
SABIC method
Linear Mold Shrinkage, Transverse
0.0060
-
0.0080
cm/cm
0.0060
-
0.0080
in/in
SABIC method
Melt Flow
19
g/10 min
@Load 5.00 kg,
Temperature 230 °C
19
g/10 min
@Load 11.0 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
27.0
MPa
3920
psi
50 mm/min; ASTM D638
27.0
MPa
3920
psi
50 mm/min; ISO 527
Tensile Strength, Yield
40.0
MPa
5800
psi
50 mm/min; ASTM D638
40.0
MPa
5800
psi
50 mm/min; ISO 527
Elongation at Break
14.6 %
14.6 %
50 mm/min; ASTM D638
17.9 %
17.9 %
50 mm/min; ISO 527
Elongation at Yield
3.6 %
3.6 %
50 mm/min; ISO 527
3.7 %
3.7 %
50 mm/min; ASTM D638
Tensile Modulus
1.80
GPa
261
ksi
1 mm/min; ISO 527
1.90
GPa
276
ksi
50 mm/min; ASTM D638
Flexural Strength
56.0
MPa
8120
psi
2 mm/min; ISO 178
59.0
MPa
8560
psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus
1.80
GPa
261
ksi
2 mm/min; ISO 178
1.90
GPa
276
ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched
91.0
J
67.1
ft-lb
ASTM D256
Izod Impact, Unnotched
10.66
J/cm
19.97
ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO)
12.0
kJ/m²
5.71
ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO)
135
kJ/m²
64.2
ft-lb/in²
80*10*4; ISO 180/1U
Electrical Properties
Metric
English
Comments
Surface Resistance
1.00e+10
-
1.00e+12
ohm
1.00e+10
-
1.00e+12
ohm
ASTM D257
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
100
µm/m-°C
@Temperature 23.0 - 60.0 °C
55.6
µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow
110
µm/m-°C
@Temperature 23.0 - 60.0 °C
61.1
µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi)
92.0
°C
198
°F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
90.0
°C
@Thickness 3.20 mm
194
°F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
81.0
°C
178
°F
Flatw 80*10*4 sp=64mm; ISO 75/Af
75.0
°C
@Thickness 3.20 mm
167
°F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point
94.0
°C
201
°F
Rate B/50; ISO 306
95.0
°C
203
°F
Rate B/120; ISO 306
Processing Properties
Metric
English
Comments
Zone 2
195
-
205
°C
383
-
401
°F
Zone 3
205
-
215
°C
401
-
419
°F
Melt Temperature
200
-
210
°C
392
-
410
°F
Injection Molding
Mold Temperature
10.0
-
50.0
°C
50.0
-
122
°F
Drying Temperature
70.0
-
80.0
°C
158
-
176
°F
Injection Molding
Dry Time
4.00
hour
4.00
hour
Injection Molding
Back Pressure
0.200
-
0.300
MPa
29.0
-
43.5
psi
Screw Speed
30
-
60
rpm
30
-
60
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PSABH81407 / 289354
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.