The AMPC100P product is a general purpose polycarbonate powder for additive manufacturing via selective laser sintering process. Made with LEXAN™ resin, it is white in appearance and offers a combination of good mechanical properties and high temperature resistance that make it suitable for a variety of industrial applications. The AMPC100P powder is compatible with most common SLS printers, and can be recycled up to 100%. Information provided by SABIC |