MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Materion Niobium Oxide (NbOx)™ Rotatable Sputtering Target for Glass & Display Applications
Categories: Ceramic; Oxide

Material Notes: Materion supplies rotatable sputtering targets. Our target products for Niobium Oxide (NbOx) coatings are particularly suited for glass and display applications. Achieving optimal results during the deposition process requires cylindrical targets that are capable of consistently producing uniform thin films that meet or exceed industry standards. Our rotatable sputtering targets are specifically developed to produce low defect films for large area coating operations with optimized target life time.

Benefits

  • Longer target life time reduces downtime for change outs and chamber maintenance
  • Increased material utilization
  • Pure NbOx with optimized microstructure for best homogeneity and sputtering performance on full target volume
  • Custom designed special geometries available

Information provided by Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density >= 4.90 g/cc
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity <= 0.300 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 2.78 µin/in-°F
Thermal Conductivity 2.50 W/m-K
Melting Point 1500 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMATER910 / 323523

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.