MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Epoxies, Etc 50-3182 NC Thermally Conductive Epoxy Resin
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: 50-3182 NC is a highly filled epoxy system with excellent physical, electrical, and thermal properties. 50-3182 NC offers very high thermal conductivity, excellent electrical insulation, and low thermal expansion. This unique combination of properties makes this system ideal for applications where electrical insulation and mechanical protection must be maintained while transferring heat.

Applications: 50-3182 NC is ideal for high voltage applications such as power supplies, transformers, high voltage insulators, bushings, etc.

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.30 g/cc2.30 g/cc
Water Absorption 0.11 %
@Time 605000 sec
0.11 %
@Time 168 hour
Viscosity 15000 cP15000 cPCat.140
 45000 cP45000 cPCat.30
 90000 cP90000 cPCat.190
Linear Mold Shrinkage 0.0010 cm/cm0.0010 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9595
Tensile Strength 58.6 MPa8500 psi
Flexural Strength 93.1 MPa13500 psi
Flexural Modulus 1.72 GPa250 ksi
Compressive Strength 117 MPa17000 psi
Compressive Modulus 10.3 GPa1500 ksiElastic
Izod Impact, Notched 0.187 J/cm0.350 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.90e+16 ohm-cm4.90e+16 ohm-cm
Dielectric Constant 6.4
@Frequency 60 Hz
6.4
@Frequency 60 Hz
Dielectric Strength 22.0 kV/mm560 kV/in
Dissipation Factor 0.018
@Frequency 60 Hz
0.018
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 1.66 W/m-K11.5 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 205 °C401 °F
Heat Distortion Temperature 175 °C347 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFEPOX056 / 316733

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.