MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Radici Radiflam® B RV300K AE 375 BK Polybutylene Terephthalate
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: PBT flame retardant, injection molding grade. 30% glass fiber reinforced. Black color.

Suitable for parts requiring fire retardancy along with high stiffness and good mechanical resistance.

Information provided by Radici Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.66 g/cc0.0600 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm0.0090 in/inISO 294-4
Melt Flow 3.5 g/10 min
@Load 2.16 kg,
Temperature 250 °C
3.5 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 130 MPa18900 psi5mm / min.; ISO 527-2/1A
Elongation at Break 2.2 %2.2 %5 mm / min.; ISO 527-2/1A
Tensile Modulus 10.7 GPa1550 ksi1mm / min.; ISO 527-2/1A
Flexural Strength 205 MPa29700 psi2mm / min.; ISO 178
Flexural Modulus 9.70 GPa1410 ksi2mm / min.; ISO 178
Charpy Impact Unnotched 6.00 J/cm²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1e/A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cm500V; IEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohm500V; IEC 60093
Comparative Tracking Index 250 V250 VSol.A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FISO 75/2Af
Vicat Softening Point 210 °C
@Load 5.10 kg
410 °F
@Load 11.2 lb
50°C/h; ISO 306
Flammability, UL94  V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
 V-0
@Thickness 0.400 mm
V-0
@Thickness 0.0157 in
Flame Spread 0.000 mm/min
@Thickness 3.00 mm
0.000 in/min
@Thickness 0.118 in
Automotive Interior; ISO 3795
Glow Wire Flammability Index  960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
IEC 60695-2-1/2
 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
IEC 60695-2-1/2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 280 °C482 - 536 °FInjection Molding
Mold Temperature 80.0 - 90.0 °C176 - 194 °F
 
Descriptive Properties
Injection Molding Injection SpeedMedium-high

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRADI6986 / 293491

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.