MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Mitsubishi CPX Low-Warp Polypropylene 3D Printing Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: CPX is a low warp Polypropylene with good layer adhesion and extreme toughness. Co-Developed with Filament Innovations, CPX is most typically used for the prosthetic market, but also has been proven to create extremely tough parts for functional use in industrial and medical applications.

Material features:

  • Good flexibility
  • Extremely stiff
  • Excellent impact resistance
  • Good layer adhesion
Colors: CPX is available in natural and black colors.

Information provided by Mitsubishi Chemical.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.900 g/cc0.900 g/ccISO 1183
Filament Diameter 1750 µm1750 µm>95% Roundness
 2850 µm2850 µm>95% Roundness
Melt Flow 0.400 g/10 min0.400 g/10 min ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 15.1 MPa2190 psiISO 527
Tensile Strength, Yield 19.5 MPa2830 psiISO 527
Elongation at Break 100 %100 %ISO 527
Elongation at Yield 17 %17 %ISO 527
Flexural Modulus 0.810 GPa117 ksiISO 178
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 - 240 °C428 - 464 °FISO 527
 
Processing PropertiesMetricEnglishComments
Processing Temperature 240 - 260 °C464 - 500 °FPrinting Nozzle Temperature
 
Descriptive Properties
Bed MaterialPEI w/BuildTak Bond for PP
Bed Temp85-90°C
Nozzle Diameter0.25 - 0.6 mm
Print Speed25 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMITS9803m / 322772

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.