MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper Alloy, UNS C27250, H02 Temper; Rod, Bar & Forging
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: 1/2 Hard

Fabrication Properties: Excellent Suitability – Soldering; Good Suitability – Brazing, Spot Weld, Capacity for Being Cold Worked; Fair Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Butt Weld, Capacity for Being Hot Formed

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.17 g/cc0.295 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 5656
Tensile Strength >= 310 MPa>= 45000 psi
 338 MPa49000 psiTypical
Tensile Strength, Yield >= 172 MPa>= 25000 psi0.5% Ext
 207 MPa30000 psi0.5% Ext, Typical
Elongation at Break >= 13 %>= 13 %
 26 %26 %Typical
Modulus of Rigidity 39.6 GPa5750 ksi
Machinability 90 %90 %
Forgeability 80 %80 %
Impact Test 16.3 J12.0 ft-lb
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000820 ohm-cm0.00000820 ohm-cm21% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 21.6 µm/m-°C
@Temperature 20.0 - 300 °C
12.0 µin/in-°F
@Temperature 68.0 - 572 °F
 
Component Elements PropertiesMetricEnglishComments
Bismuth, Bi <= 0.0090 %<= 0.0090 %
Carbon, C 0.20 - 1.2 %0.20 - 1.2 %
Copper, Cu 62 - 65 %62 - 65 %
Iron, Fe <= 0.35 %<= 0.35 %
Lead, Pb <= 0.0090 %<= 0.0090 %
Phosphorus, P 0.050 - 0.40 %0.050 - 0.40 %
Silicon, Si <= 0.0090 %<= 0.0090 %
Zinc, Zn 33.4 - 37.8 %33.4 - 37.8 %As Balance

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC27250x1 / 291838

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.