MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Alliance BIF-14 Bonded Injection Ferrite Magnet
Categories: Ceramic; Oxide; Metal; Electronic/Magnetic Alloy

Material Notes: Bonded Magnets are custom designed and made with an infinite selection of materials, grades and shapes. Ferrite Bonded Magnets that utilize an injection molding processes can be made by combining a variety of Ferrite powders with Nylon 6, Nylon 12, PPS and other resins. The ratios between magnetic powders and resins are endless, therefore many grades exist depending on magnetic performance, temperature resistance, and mechanical strength. These materials can be molded directly over or into another polymer or metal component. The shapes and sizes are endless, as are the magnetization patterns that can be achieved either in the molding tool or by utilizing a magnetizing fixture.

Information provided by Alliance LLC.

Key Words: Permanent Magnet
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 3.60 - 3.80 g/cc
Water Absorption 0.020 - 0.050 %PPS
 0.050 - 3.2 %PA12
 0.30 - 11 %PA6
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 92 - 133
Tensile Strength, Yield 20.0 - 142 MPaPA6
 13.0 - 150 MPaPPS
 13.0 - 171 MPaPA12
 
Electrical PropertiesOriginal ValueComments
Magnetic Coercive Force, Hc 2200 - 2510 Oe
 2760 - 3270 OeIntrinsic
Magnetic Remanence, Br 2550 - 2800 Gauss
Magnetic Maximum Energy Product, BH 1.6 - 1.9 MGOe
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air <= 120 °CPA12
 <= 150 °CPA6
 <= 180 °CPPS
 
Processing PropertiesOriginal ValueComments
Mold Temperature 20.0 - 120 °CPA12
 70.0 - 150 °CPA6
 135 - 175 °CPPS
 
Descriptive Properties
Reversible Temperature Coefficients-0.18Bd. %/°C
 0.4Hd. %/°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NALLIAN76t / 268413

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.