MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Nouryon Trigonox C Polymer Crosslinking tert-Butyl peroxybenzoate
Categories: Other Engineering Material

Material Notes: Trigonox C is a pure peroxide in liquid form.

CAS number: 614-45-9

EINECS/ELINCS No: 210-382-2

Applications: Polymerization of styrene: Trigonox C may be used for the (co)polymerization of styrene in the temperature range of 100- 140°C. In practice, combinations of two or more peroxides with diverging activities are used to reduce the residual monomer content in the final polymer and to increase reactor efficiency. Polymerization of ethylene: Trigonox C is an efficient initiator for the ethylene polymerization at high pressure in both autoclave and tubular processes. To obtain a wide spectrum of polymerization temperatures, Trigonox C is often used in combination with other peroxides. Depending on reaction conditions, Trigonox C is active in the temperature range of 220-270°C. Polymerization of acrylates and methacrylates: Trigonox C may be used as an initiator for the bulk, suspension and solution (co)polymerization of acrylates and methacrylates in the temperature range of 90-130°C. For Thermoset: Trigonox C, tert-butyl peroxybenzoate, is an aromatic perester, which is used for the curing of unsaturated polyester resins at elevated temperatures. Trigonox C is preferred for the curing of UP resin based Hot Press Moulding formulations (SMC, BMC etc.) in the temperature range of 120-170°C. Trigonox C can also be used in combination with high reactive peroxides like Perkadox 16 or Trigonox HMa as kicker in formulations for pultrusion in the temperature range of 100-150°C. In combination with a cobalt accelerator (e.g. Accelerator NL-53N, 10% cobalt), Trigonox C is also applicable for the cure of UP resins in the temperature range of 70°C and higher. Application area can be: air drying lacquers, diplacquers, filament winding, etc. For Crosslinking: Trigonox C is a monofunctional peroxide which is used for the crosslinking of natural rubber and synthetic rubbers, as well as polyolefins. Safe processing temperature: 100°C (rheometer ts2 > 20 min.). Typical crosslinking temperature: 140°C (rheometer t90 about 12 min.).

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Half-life  0.100
@Temperature 142 °C
0.100
@Temperature 288 °F
[hr]
 1.00
@Temperature 122 °C
1.00
@Temperature 252 °F
[hr]
 10.0
@Temperature 103 °C
10.0
@Temperature 217 °F
[hr]
Molecular Weight 194.2 g/mol194.2 g/mol
Storage Temperature 10.0 - 25.0 °C50.0 - 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 60.0 °C140 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceClear liquid
Assay= 98.0 %
Content (%)8.24Active oxygen content peroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY1169 / 286692

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.