MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Cadmium Copper, UNS C16200, H04 Temper, Flat Products, Rod & Bar
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Hard

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Capacity for Being Cold Worked; Good Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Butt Weld, Capacity for Being Hot Formed

Common Fabrication Processes: Drawing; Etching; Forming and Bending; Heading and Upsetting; Hot forging; Piercing; Punching

Typical uses: Electric Blanket Elements; Cable Wrap; Clamps; Connectors; Contacts; Current Carrying Rings; Fittings; Fuse Clips; Heating Pad Elements; High Strength Transmission Lines; Rail bands; Resistance and Spot Welding Electrodes; Spring Contacts; Switch Gear; Tinsel for the Telephone Industry; Trolley Wire; Wave Guide Cavities; Wire for Telephone Cord Sets Back Up Bars; Resistance Welding Tips; Structural Parts in Resistance Welding Machines

Applicable Specifications: Bar- SAE J461, SAE J463; Forgings – SAE J463, Forgings SAE J461; Rod – SAE J463, SAE J461; Wire – ASTM B105, MILITARY MIL-W-82598, ASTM B624

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.321 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 60.0 ksi
@Thickness 1.02 mm
 70.0 ksi
@Thickness 2.03 mm
 73.0 ksi
@Thickness 12.7 mm
Tensile Strength, Yield 45.0 ksi
@Thickness 1.02 mm
0.5% Ext
 55.0 ksi
@Thickness 2.03 mm
0.5% Ext
 69.0 ksi
@Thickness 12.7 mm
0.5% Ext
Elongation at Break 5.0 %
@Thickness 1.02 mm
 6.0 %
@Thickness 2.03 mm
 9.0 %
@Thickness 12.7 mm
Tensile Modulus 17000 ksi
Modulus of Rigidity 6400 ksi
Poissons Ratio 0.33Calculated
Machinability 20 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000191 ohm-cm90% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.40 µin/in-°F
@Temperature 20.0 - 100 °C
 9.60 µin/in-°F
@Temperature 20.0 - 200 °C
 9.80 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 208 BTU-in/hr-ft²-°F
Melting Point 1886 - 1969 °F
Solidus 1886 °F
Liquidus 1969 °F
Annealing Point 800 - 1400 °F
 
Processing PropertiesOriginal ValueComments
Hot-Working Temperature 1400 - 1600 °F
 
Component Elements PropertiesOriginal ValueComments
Cadmium, Cd 0.70 - 1.2 %
Copper, Cu 98.8 - 99.3 %As Balance
Iron, Fe <= 0.020 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC16200x2 / 292811

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.