MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Corning RSG 32 Nuclear Shielding Leaded Glass Block
Categories: Ceramic; Glass

Material Notes: Corning supplies glass blocks for radiation-shielding windows. Individual blocks can weigh in excess of 4000 kgs and are some of the largest pieces of glass produced worldwide, enabling a wide range of applications in its finished form. Corning manufactures raw blocks which are supplied to Sovis Optique, who cut and polish to customer specific sizes. RSG 32 is available with added gadolinium for extra neutron attenuation.

Information provided by Corning Incorporated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.22 g/cc
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.584
 
Component Elements PropertiesOriginal ValueComments
CeO2 1.6 - 1.8 %
Lead, Pb 30.6 %33 wt% PbO
 
Descriptive Properties
PbO Content (%)33

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Schott Glass 8095 Lead Glass
Corning RWG 52 Nuclear Shielding Leaded Glass Block
Corning RW 36 Nuclear Shielding Leaded Glass Block
Corning RSG 52 Nuclear Shielding Leaded Glass Block

CCORNG984 / 233280

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.