SABIC CYCOLOY™ FR C4210HF PC+ABS (Americas)
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Polycarbonate/ABS Alloy, Unreinforced
Material Notes:
PC+ABS Blend with 10% Glass Reinforce. High flow, High heat resistance., Excellent balance strength/rigidity. Good impact/appearance.
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.22
g/cc
1.22
g/cc
ASTM D792
Linear Mold Shrinkage, Flow
0.0030
-
0.0050
cm/cm
@Thickness 3.20 mm
0.0030
-
0.0050
in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse
0.0030
-
0.0050
cm/cm
@Thickness 3.20 mm
0.0030
-
0.0050
in/in
@Thickness 0.126 in
SABIC method
Melt Flow
37
g/10 min
@Load 5.00 kg,
Temperature 260 °C
37
g/10 min
@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell R
121
121
ISO 2039-2
Ball Indentation Hardness
116
MPa
16800
psi
ISO 2039-1
Tensile Strength at Break
85.0
MPa
12300
psi
5 mm/min; ASTM D638
90.0
MPa
13100
psi
5 mm/min; ISO 527
Tensile Strength, Yield
85.0
MPa
12300
psi
5 mm/min; ASTM D638
90.0
MPa
13100
psi
5 mm/min; ISO 527
Elongation at Break
3.0 %
3.0 %
5 mm/min; ASTM D638
3.2 %
3.2 %
5 mm/min; ISO 527
Elongation at Yield
3.0 %
3.0 %
5 mm/min; ASTM D638
Tensile Modulus
4.70
GPa
682
ksi
1mm/min; ISO 527
4.90
GPa
711
ksi
5 mm/min; ASTM D638
Flexural Strength
135
MPa
19600
psi
2 mm/min; break; ISO 178
140
MPa
20300
psi
brk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Yield Strength
125
MPa
18100
psi
2 mm/min; ISO 178
Flexural Modulus
4.25
GPa
616
ksi
2 mm/min; ISO 178
4.30
GPa
624
ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched
0.750
J/cm
1.41
ft-lb/in
ASTM D256
0.600
J/cm
@Temperature -30.0 °C
1.12
ft-lb/in
@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched
4.80
J/cm
8.99
ft-lb/in
ASTM D4812
4.80
J/cm
@Temperature -30.0 °C
8.99
ft-lb/in
@Temperature -22.0 °F
ASTM D4812
Izod Impact, Notched (ISO)
8.00
kJ/m²
3.81
ft-lb/in²
80*10*4; ISO 180/1A
6.00
kJ/m²
@Temperature -30.0 °C
2.86
ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO)
30.0
kJ/m²
14.3
ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy
15.0
J
11.1
ft-lb
ASTM D3763
8.00
J
@Temperature -30.0 °C
5.90
ft-lb
@Temperature -22.0 °F
ASTM D3763
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
40.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
22.2
µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow
75.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
41.7
µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Thermal Conductivity
0.200
W/m-K
1.39
BTU-in/hr-ft²-°F
ISO 8302
Deflection Temperature at 0.46 MPa (66 psi)
134
°C
@Thickness 3.20 mm
273
°F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
126
°C
@Thickness 3.20 mm
259
°F
@Thickness 0.126 in
unannealed; ASTM D648
128
°C
@Thickness 6.40 mm
262
°F
@Thickness 0.252 in
unannealed; ASTM D648
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PSABI10781 / 244248
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.