MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Akro-Plastic Akromid® A3 5 S3 black (7333) Unreinforced Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Heat Stabilized

Material Notes: Unreinforced. Heat stabilized material, dry impact. PA 6.6-I.

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.013 - 0.015 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.015 - 0.017 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 50.0 MPa50 mm/min; Conditioned; ISO 527-2
 70.0 MPa50 mm/min; Dry as Molded; ISO 527-2
Elongation at Break >= 25 %50 mm/min; Dry as Molded; ISO 527-2
 >= 80 %50 mm/min; Conditioned; ISO 527-2
Tensile Modulus 1200 MPa1 mm/min. Conditioned; ISO 527-2
 2300 MPa1 mm/min. Dry as Molded.; ISO 527-2
Charpy Impact Unnotched NB
@Temperature 23.0 °C
Dry as molded; ISO 179-1/1eA
 NB
@Temperature 23.0 °C
Conditioned; ISO 179-1/1eA
Charpy Impact, Notched 14.0 kJ/m²
@Temperature 23.0 °C
Dry as Molded; ISO 179-1/1eA
 90.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179-1/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 262 °CDry as Molded. DES, 10°C/min; DIN EN 11357-1
Maximum Service Temperature, Air 129 °C50% Loss of Tensile Strength. IEC 60216. 5000h
Flammability, UL94 HB
@Thickness 1.60 mm
Conditioned
 HB
@Thickness 1.60 mm
Dry as Molded
 
Descriptive Properties
Burning Rate<100 mm/minDry as Molded. FMVSS 302. >1 mm thickness
 <100 mm/minConditioned. FMVSS 302. >1 mm thickness

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKRO9802 / 255459

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.