MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Master Bond EP40TCMed Two component, thermally conductive, electrically insulative epoxy system
Categories: Polymer; Thermoset; Epoxy; Epoxy, Thermally Conductive

Material Notes: Key Features:
  • Convenient handling
  • Excellent toughness
  • Superior bond strength
  • Passes ISO 10993-5 specifications
Product Description: Master Bond EP40TCMed is a two component, thermally conductive, electrically isolating epoxy for bonding and sealing. It combines convenient processing with superior strength properties after curing. It is a moderate viscosity, flowable system with a forgiving 1 to 1 mix ratio by weight or volume, and a user friendly working life. EP40TCMed cures readily at ambient temperatures or more rapidly with heat. The optimum cure schedule is overnight at room temperature followed by 3-5 hours at 125°F to 150°F. The system has no solvents or diluents and offers low shrinkage upon curing. This epoxy bonds well to a wide range of substrates including metals, ceramics, composites and many plastics. Most compelling is its exceptionally high shear and peel strength. EP40TCMed has remarkable toughness as indicated by its high elongation of 60-70%. This translates into the ability to withstand the most rigorous thermal cycling as well as vibration and shock. It is able to transfer heat, without conducting electricity. The ability to transfer heat is enhanced by the exceptionally small particle size of the filler used in this system. The average particle size is 3-4 microns, the largest is 14 microns (<1%). The net effect is to allow for thinner bond lines and lower thermal resistance values. This system resists many chemicals including water, oils, fuels and most notably, EtO, radiation and several cold sterilants. The color of Part A is light gray and Part B is gray. The service temperature range is -100°F to +300°F. EP40TCMed should be considered in medical device assembly applications where a thermally conductive, electrically insulating, biocompatible epoxy is needed.

Product Advantages:

  • Easy processing, 1:1 mix ratio
  • Long open time
  • Outstanding shear and peel strength
  • Very high elongation
  • Resists sterilization

Information provided by Master Bond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 40000 - 80000 cP40000 - 80000 cPPart B, thixotropic
 80000 - 100000 cP80000 - 100000 cPMixed
 150000 - 250000 cP150000 - 250000 cPPart A, thixotropic
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 70 - 8070 - 80
Tensile Strength 6.89 - 13.8 MPa1000 - 2000 psi
Elongation at Break 60 - 70 %60 - 70 %
Tensile Modulus 0.0345 - 0.103 GPa5.00 - 15.0 ksi
Adhesive Bond Strength 15.9 - 17.2 MPa2300 - 2500 psiTensile lap shear, Al to Al
Peel Strength 7.01 - 10.5 kN/m40.0 - 60.0 pliT-peel strength, steel to steel
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Dielectric Constant 4.4
@Frequency 60 Hz
4.4
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 40.0 - 45.0 µm/m-°C22.2 - 25.0 µin/in-°F
Thermal Conductivity 1.15 - 1.59 W/m-K8.00 - 11.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -73.3 °C-100 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  180 - 300 min
@Temperature 51.7 - 65.6 °C
3.00 - 5.00 hour
@Temperature 125 - 150 °F
Optimal: overnight at 75°F, plus 3-5 hours at 125-150°F
 2880 - 4320 min
@Temperature 23.9 °C
48.0 - 72.0 hour
@Temperature 75.0 °F
Option 2
Working Life 120 - 180 min120 - 180 minafter mixing, 100 gram batch
Shelf Life 6.00 Month6.00 Monthin original, unopened containers
 
Descriptive Properties
Mixing ratio1:1 by weight or volumePart A to B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMASTM5923 / 306812

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.