Krytox™ EG 3000 grease is formulated specifically for electrical applications. While this grade offers different viscosities to match the application in which it is being used, it is: Clear, colorless, fluorinated synthetic greases, Nonreactive and nonflammable, Safe in environments with chemical and oxygen service, Long lasting.Information provided by Chemours Krytox |