MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Angst+Pfister APSOplast® PPS GF40 PPS + 40% glass fibre
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler

Material Notes: This semi-crystalline polymer is filled with 40% glass fibre. It has exceptional rigidity and hardness, even at a service temperature of up to +220 °C. Its very good chemical resistance, low creep tendency, and high dimensional stability allow applications for components with high thermal and mechanical stresses in the fields of pumps, fittings, chemical plants, and mechanical engineering. This material is also used for small high-precision parts with high dimensional stability in the electrical and nuclear industries. This glass fibre filled PPS does, however, tend to have brittle-like breaking behavior.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.65 g/ccDIN EN ISO 1183-1
Water Absorption <= 0.010 %
@Time 346000 sec
DIN EN ISO 62
 0.015 %
@Time 86400 sec
DIN EN ISO 62
Moisture Absorption 0.0150 %at saturation in standardized climate; DIN EN ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 92DIN EN ISO 868
Ball Indentation Hardness 250 MPaDIN EN ISO 2039-1
Tensile Strength, Yield 90.0 MPaDIN EN ISO 527
Elongation at Break 2.0 %DIN EN ISO 527
Modulus of Elasticity 6.50 GPaDIN EN ISO 527
Charpy Impact Unnotched 24.0 kJ/m²DIN EN ISO 179-1eU
 
Thermal PropertiesOriginal ValueComments
CTE, linear 30.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
Melting Point 285 °CISO 11357-3
Maximum Service Temperature, Air 220 °Clong term
 250 °Cshort term
Deflection Temperature at 1.8 MPa (264 psi) 260 °CDIN EN ISO 75 / A
Minimum Service Temperature, Air 0.000 °C
Flammability, UL94 V-0
@Thickness 3.00 mm
 V-0
@Thickness 6.00 mm
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PANGP056 / 250554

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.