MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Epoxies, Etc 20-3001 NC Epoxy Potting And Encapsulating Resin
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Description: 20-3001 NC is a low viscosity, unfilled epoxy potting and encapsulating system which forms a bubble free glass like finish when cured. This is a 100% solids resin system that does not contain any solvents. Its convenient 1:1 mix ratio and lack of fillers make it an ideal material for meter mix and dispense equipment. 20-3001 NC has been formulated for ease in handling. Its low viscosity aids in filling voids and air pockets. In addition, there is no filler settling with this system. 20-3001 NC is the non-crystallizing version of the original 20-3001 product.

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.12 g/cc1.12 g/cc
Viscosity 1000 cP1000 cPMixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565
Tensile Strength 39.3 MPa5700 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.00e+15 ohm-cm5.00e+15 ohm-cm
Dielectric Constant 4.7
@Frequency 60 Hz
4.7
@Frequency 60 Hz
Dielectric Strength 22.0 kV/mm558 kV/in
Dissipation Factor 0.034
@Frequency 60 Hz
0.034
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 50.0 µm/m-°C27.8 µin/in-°F
Thermal Conductivity 0.430 W/m-K2.98 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Processing PropertiesMetricEnglishComments
Pot Life 20.0 min
@Load 0.100 kg
20.0 min
@Load 0.221 lb
 
Descriptive Properties
ColorBlack or Clear
Mix Ratio1:1by volume
 100:83by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFEPOX022 / 316699

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.