MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

BASF Ultrason® P 3010 PPSU
Categories: Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes: Ultrason P 2010 is an unreinforced, medium viscosity injection molding PPSU grade

Information provided by BASF.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.29 g/cc0.0466 lb/in³ISO 1183
Moisture Absorption 0.600 %0.600 %50% RH; ISO 62
Water Absorption at Saturation 1.2 %1.2 %ISO 62
Linear Mold Shrinkage, Flow 0.0090 cm/cm0.0090 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/inISO 294-4
Melt Flow 35 g/10 min
@Load 10.0 kg,
Temperature 360 °C
35 g/10 min
@Load 22.0 lb,
Temperature 680 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 124 MPa18000 psiISO 2039-1
Tensile Strength, Yield 74.0 MPa10700 psiISO 527
Elongation at Yield 7.8 %7.8 %ISO 527
Tensile Modulus 2.27 GPa329 ksiISO 527
Izod Impact, Notched (ISO)  25.0 kJ/m²
@Temperature -30.0 °C
11.9 ft-lb/in²
@Temperature -22.0 °F
ISO 180
 55.0 kJ/m²
@Temperature 23.0 °C
26.2 ft-lb/in²
@Temperature 73.4 °F
ISO 180
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched  2.50 J/cm²
@Temperature -30.0 °C
11.9 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 7.50 J/cm²
@Temperature 23.0 °C
35.7 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmIEC 60093
Dielectric Constant  3.7
@Frequency 1e+6 Hz
3.7
@Frequency 1e+6 Hz
IEC 60250
 3.8
@Frequency 100 Hz
3.8
@Frequency 100 Hz
IEC 60250
Dielectric Strength 44.0 kV/mm1120 kV/inIEC 60243-1
Dissipation Factor  0.017
@Frequency 100 Hz
0.017
@Frequency 100 Hz
IEC 60250
 0.089
@Frequency 1e+6 Hz
0.089
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 150 V150 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 55.0 µm/m-°C30.6 µin/in-°F
Deflection Temperature at 1.8 MPa (264 psi) 198 °C388 °FISO 75
Flammability, UL94  V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 350 - 390 °C662 - 734 °F
Mold Temperature 140 - 180 °C284 - 356 °F
Drying Temperature 130 - 150 °C
@Time 14400 sec
266 - 302 °F
@Time 4.00 hour
Moisture Content <= 0.020 %<= 0.020 %
Injection Pressure 3.45 - 10.3 MPa500 - 1500 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASF8989 / 254947

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.