MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Epoxies, Etc 10-3062 Epoxy Adhesive
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: 10-3062 is a room temperature curing, two component, epoxy potting compound and adhesive. The 10-3062 provides good water resistance, adhesion, and toughness. It is packaged in the convenient TriggerBond™ dual barrel cartridge system. The 10-3062 Epoxy System meets the Food and Drug Administration (FDA) regulations permitting use in “indirect” food contact applications. The raw materials used in the products comply with the FDA regulations of Title 21 Code of Federal Regulations under Sections 175.105 and 175.300.

Benefits:

  • Excellent adhesion
  • Excellent chemical and corrosion resistance
  • Excellent electrical insulation

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.09 g/cc1.09 g/cc
Viscosity 24000 cP24000 cPMixed
Storage Temperature 10.0 - 25.0 °C50.0 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8282
Tensile Strength 57.2 MPa8300 psi
Elongation at Break 4.9 %4.9 %
Flexural Strength 95.1 MPa13800 psi
Flexural Modulus 2.14 GPa310 ksi
Compressive Strength 228 MPa33000 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.70e+15 ohm-cm1.70e+15 ohm-cm
Dielectric Constant 2.7
@Frequency 120 Hz
2.7
@Frequency 120 Hz
Dissipation Factor 0.0030
@Frequency 120 Hz
0.0030
@Frequency 120 Hz
 
Processing PropertiesMetricEnglishComments
Cure Time  15.0 min
@Temperature 104 °C
0.250 hour
@Temperature 219 °F
 60.0 min
@Temperature 66.0 °C
1.00 hour
@Temperature 151 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 120 min
@Load 0.100 kg
120 min
@Load 0.221 lb
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
ColorAmberCuring Agent
 ClearResin
Mix Ratio100:50by volume (Resin : Curing Agent)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFEPOX081 / 316758

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.