MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC GELOY™ HRA222F ASA (Asia)
Categories: Polymer; Thermoplastic; ASA Polymer

Material Notes: PC/ASA flame retardant, excellent weatherability.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³ISO 1183
Water Absorption 0.60 %0.60 %23°C/sat; ISO 62
Moisture Absorption 0.200 %0.200 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inSABIC method
Melt Flow 13 g/10 min
@Load 2.16 kg,
Temperature 260 °C
13 g/10 min
@Load 4.76 lb,
Temperature 500 °F
cm³/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 45.0 MPa6530 psi50 mm/min; ISO 527
 51.0 MPa7400 psi5 mm/min; ISO 527
 56.0 MPa8120 psi50 mm/min; ASTM D638
 66.0 MPa9570 psi5 mm/min; ASTM D638
Tensile Strength, Yield 59.0 MPa8560 psi5 mm/min; ASTM D638
 60.0 MPa8700 psi50 mm/min; ISO 527
 62.0 MPa8990 psi5 mm/min; ISO 527
 63.0 MPa9140 psi50 mm/min; ASTM D638
Elongation at Break >= 50 %>= 50 %50mm/min; ISO 527
 >= 50 %>= 50 %5 mm/min; ISO 527
 >= 100 %>= 100 %50mm/min; ASTM D638
 >= 100 %>= 100 %5 mm/min; ASTM D638
Elongation at Yield 4.2 %4.2 %5 mm/min; ASTM D638
 4.3 %4.3 %50 mm/min; ASTM D638
 4.3 %4.3 %5 mm/min; ISO 527
 4.4 %4.4 %50 mm/min; ISO 527
Tensile Modulus 2.52 GPa365 ksi1mm/min; ISO 527
 2.59 GPa376 ksi5 mm/min; ASTM D638
Flexural Yield Strength 93.0 MPa13500 psi2 mm/min; ISO 178
Flexural Modulus 2.51 GPa364 ksi2 mm/min; ISO 178
Izod Impact, Notched 3.85 J/cm7.21 ft-lb/inASTM D256
 2.90 J/cm
@Temperature 0.000 °C
5.43 ft-lb/in
@Temperature 32.0 °F
ASTM D256
Izod Impact, Notched (ISO) 17.0 kJ/m²8.09 ft-lb/in²80*10*4; ISO 180/1A
 9.00 kJ/m²
@Temperature -30.0 °C
4.28 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
 12.0 kJ/m²
@Temperature 0.000 °C
5.71 ft-lb/in²
@Temperature 32.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 1.50 J/cm²7.14 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VIEC 60112
 >= 600 V>= 600 VUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 69.0 µm/m-°C
@Temperature -30.0 - 80.0 °C
38.3 µin/in-°F
@Temperature -22.0 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow  71.0 µm/m-°C
@Temperature -30.0 - 80.0 °C
39.4 µin/in-°F
@Temperature -22.0 - 176 °F
ISO 11359-2
 75.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
41.7 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
Hot Ball Pressure Test 75.0 °C167 °FIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °C210 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C190 °F1.8 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 102 °C216 °FRate B/50; ISO 306
 104 °C219 °FRate B/120; ISO 306
 111 °C232 °FRate A/50; ISO 306
UL RTI, Electrical 90.0 °C194 °FUL 746B
UL RTI, Mechanical with Impact 90.0 °C194 °FUL 746B
UL RTI, Mechanical without Impact 90.0 °C194 °FUL 746B
Flammability, UL94 V-0
@Thickness 2.00 mm
V-0
@Thickness 0.0787 in
UL 94
Oxygen Index 29 %29 %ISO 4589
 
Processing PropertiesMetricEnglishComments
Processing Temperature 60.0 - 80.0 °C140 - 176 °FHopper Temperature
Nozzle Temperature 220 - 260 °C428 - 500 °FInjection Molding
Zone 1 200 - 230 °C392 - 446 °F
Zone 2 220 - 260 °C428 - 500 °F
Zone 3 230 - 270 °C446 - 518 °F
Melt Temperature 230 - 270 °C446 - 518 °F
Mold Temperature 50.0 - 70.0 °C122 - 158 °F
Drying Temperature 80.0 - 90.0 °C176 - 194 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
Moisture Content 0.020 %0.020 %
 
Descriptive Properties
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10144 / 243611

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.