MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Michelman® Michem ® Flex P1309 Water-based primer
Categories: Fluid

Material Notes: Water-based primer for polyethylene extrusion and anchor coating Michem® Flex P1309 may applied via flexo, gravure or smooth roll coater. It can be diluted 1:1 with water or with a 50:50 pre-mixture of water and isopropyl alcohol prior to use. It has good compatibility with both Ethanol & Methanol but limited compatibility in IPA solvent. It is recommended that IPA must always be diluted with water before use. It is recommended to corona or flame-treat substrates prior to priming and dry thoroughly with hot, circulating air. This product is highly recommended for application in-line to a target coat weight on film substrates of 0.025 0.075 dry g/m2. This product was specifically designed for and is available only in Asia. Usage: A primer for film, metalized film, printed film and paper substrates promoting excellent adhesion to extrusion coated resins, resulting in high bond strength for dry and low moisture content products. Michem Flex P1309 creates very strong
adhesion between treated film and PE and EVA extrudates.

Applications (properties imparted): Extrusion Coating Primers (adhesion for film, adhesion for metal and paper).

Handling: Handle in accordance with good industrial hygiene and safety practice.

Information provided by Michelman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.01 - 1.04 g/cc1.01 - 1.04 g/cc
Solids Content 4.5 - 5.5 %4.5 - 5.5 %Non-Volatiles
pH 10 - 1210 - 12
Brookfield Viscosity 0.00 - 50 cP0.00 - 50 cPSpindle #1. 60 RPM.
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 MonthDry, cool and well-ventilated place
 
Descriptive Properties
AppearanceClear liquid
Freeze/Thaw StabilityStable after 5 Cycles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WMICHE9826 / 287421

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.