MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC GELOY™ XTWM206 ASA (Americas)
Categories: Polymer; Thermoplastic; ASA Polymer

Material Notes: ASA, Xtreme weatherability, high heat.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/ccASTM D792
Density 1.09 g/ccISO 1183
Water Absorption 0.50 %23°C/sat; ISO 62
Moisture Absorption 0.200 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cmSABIC method
 0.0040 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0075 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 7.1 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ASTM D1238
 7.2 g/10 min
@Load 3.80 kg,
Temperature 280 °C
ASTM D1238
 8.8 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 9.0 g/10 min
@Load 5.00 kg,
Temperature 260 °C
cm³/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 100ASTM D785
Tensile Strength at Break 36.0 MPa5 mm/min; ASTM D638
 36.0 MPa50 mm/min; ISO 527
 37.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 43.0 MPa5 mm/min; ASTM D638
 45.0 MPa50 mm/min; ISO 527
 46.0 MPa50 mm/min; ASTM D638
Elongation at Break 26 %50 mm/min; ASTM D638
 27 %5 mm/min; ASTM D638
 36 %50 mm/min; ISO 527
Elongation at Yield 2.5 %5 mm/min; ASTM D638
 2.7 %50 mm/min; ASTM D638
 2.8 %50 mm/min; ISO 527
Tensile Modulus 2350 MPa1mm/min; ISO 527
 2360 MPa5 mm/min; ASTM D638
 2400 MPa50 mm/min; ASTM D638
Flexural Yield Strength 64.0 MPa2 mm/min; ISO 178
 74.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2380 MPa2 mm/min; ISO 178
 2450 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 210 J/mASTM D256
 35.0 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 15.0 kJ/m²80*10*4; ISO 180/1A
 3.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 11.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 36.0 JASTM D3763
 3.00 J
@Temperature -30.0 °C
ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 83.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 84.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 94.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 94.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Hot Ball Pressure Test 75.0 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 98.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 97.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 84.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 95.0 °CRate B/50; ISO 306
 98.0 °CRate B/50; ASTM D1525
 99.0 °CRate B/120; ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm
UL 94
 
Optical PropertiesOriginal ValueComments
Gloss 93 %60°; ASTM D523
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 220 - 255 °CInjection Molding
Zone 1 215 - 250 °C
Zone 2 220 - 255 °C
Zone 3 230 - 260 °C
Melt Temperature 240 - 270 °C
Mold Temperature 60.0 - 85.0 °C
Drying Temperature 85.0 - 90.0 °CInjection Molding
Dry Time 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Moisture Content 0.040 %
Back Pressure 0.300 - 1.00 MPa
Shot Size 40 - 80 %
Vent Depth 0.00380 - 0.00760 cm
Screw Speed 30 - 80 rpm
 
Descriptive Properties
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10165 / 243632

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.