Description: This is a non-corrosive, neutral cure, 1-part, RTV (Room Temperature Vulcanizing) silicone adhesive sealant. It is one in a range of Alkoxy cure products which are solvent free. It exhibits excellent primerless adhesion to many substrates and cures at room temperature when in contact with atmospheric moisture to form a tough rubber. This product will not corrode copper or its alloys and is suitable for use with electronic components. Key Features - Non corrosive
- Excellent adhesion to most substrates
- Excellent dielectric and isolating properties
- Low odor
Application: Fiber Optic CablesCured Product: 7 days at 23+/-2°C and 50+/-5% humidity Information provided by CHT Group |