This extruded PMMA-XT ED sheet has an anti-static surface coating on both sides, which reduces electrostatic charging. Dust attraction is significantly reduced, which means that cleaning is not required so frequently. This type of PMMA is particularly suitable for covering chalk, charcoal and similar drawings.Information provided by Angst + Pfister |