MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC CYCOLOY™ FR Resin CX2142ME Polycarbonate + ABS (PC+ABS) (Europe)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: CYCOLOY CX2142ME Polycarbonate/Acrylonitrile Butadiene Styrene (PC/ABS) blend is an injection moldable, high flow, non chlorinated/brominated flame retardant grade. It has a UL94 V0@1.2mm and 5VB@2.0mm flame rating. This grade has improved chemical resistance compared to standard PC/ABS blends and is a good candidate for thin wall applications and hospital/medical equipment.

Features: Hydrolytic Stability,Chemical Resistance,Flame Retardant,Thin Wall,Non-Chlorinated,Non-Brominated,Good Mold Release

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
Density 1.19 g/cc0.0430 lb/in³ISO 1183
Moisture Absorption 0.0400 %0.0400 %Injection Molding
 0.100 %0.100 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.20 %0.20 %ISO 62-1
Viscosity 21 cP
@Load 2.16 kg,
Temperature 260 °C
21 cP
@Load 4.76 lb,
Temperature 500 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0060 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 22.5 g/10 min
@Load 2.16 kg,
Temperature 260 °C
22.5 g/10 min
@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 51.0 MPa7400 psi50 mm/min; ISO 527
 54.0 MPa7830 psi50 mm/min; ASTM D638
Tensile Strength, Yield 61.0 MPa8850 psi50 mm/min; ISO 527
 64.0 MPa9280 psi50 mm/min; ASTM D638
Elongation at Break 90 %90 %50 mm/min; ASTM D638
 90 %90 %50 mm/min; ISO 527
Elongation at Yield 4.0 %4.0 %50 mm/min; ASTM D638
 4.0 %4.0 %50 mm/min; ISO 527
Tensile Modulus 2.70 GPa392 ksi1 mm/min; ISO 527
 2.90 GPa421 ksi50 mm/min; ASTM D638
Flexural Strength 100 MPa14500 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
 100 MPa14500 psiyield, 2 mm/min; ISO 178
Flexural Modulus 2.50 GPa363 ksi2 mm/min; ISO 178
 2.70 GPa392 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 600 J443 ft-lbASTM D256
 120 J
@Temperature -30.0 °C
88.5 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 15.0 kJ/m²7.14 ft-lb/in²80*10*3; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
80*10*3; ISO 180/1A
Charpy Impact, Notched 1.50 J/cm²7.14 ft-lb/in²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 63.0 J46.5 ft-lbASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
41.7 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
41.7 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
41.7 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
41.7 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°FISO 8302
Hot Ball Pressure Test 75.0 °C167 °FPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi)  94.0 °C
@Thickness 3.20 mm
201 °F
@Thickness 0.126 in
unannealed; ASTM D648
 98.0 °C
@Thickness 6.40 mm
208 °F
@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C183 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 84.0 °C
@Thickness 3.20 mm
183 °F
@Thickness 0.126 in
unannealed; ASTM D648
 90.0 °C
@Thickness 6.40 mm
194 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 102 °C216 °FRate B/50; ASTM D1525
 102 °C216 °FRate B/120; ISO 306
 102 °C216 °FRate B/50; ISO 306
UL RTI, Electrical 90.0 °C194 °FUL 746B
UL RTI, Mechanical with Impact 90.0 °C194 °FUL 746B
UL RTI, Mechanical without Impact 90.0 °C194 °FUL 746B
Flammability, UL94  V-0
@Thickness >=1.20 mm
V-0
@Thickness >=0.0472 in
UL 94
 5VB
@Thickness >=2.00 mm
5VB
@Thickness >=0.0787 in
UL 94
 5VA
@Thickness >=3.00 mm
5VA
@Thickness >=0.118 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 245 - 275 °C473 - 527 °F
Zone 2 220 - 265 °C428 - 509 °F
Zone 3 245 - 275 °C473 - 527 °F
Melt Temperature 245 - 275 °C473 - 527 °FInjection Molding
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 - 90.0 °C176 - 194 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 30 - 80 %30 - 80 %
Vent Depth 0.00380 - 0.00760 cm0.00150 - 0.00299 in
Screw Speed 40 - 70 rpm40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80021 / 287968

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.