OKULEN® 2000-GB is enhanced with a glass filler which gives the UHMW-PE (9 mio. g/mol) a higher abrasion resistance than standard material. It offers excellent impact strength for tough applications. Properties: Extremely wear resistant; Good sliding properties; Good chemical resistance; Low maintenance; Longer life time over standard UHMW-PE; EU 1935/2004 & 10/2011 – conform; FDA – conform Color: yellow green FN6754 Range of applications: Machine construction; Conveying industry; Agriculture, farming equipment; Waste water and filtration systems; Paper industry (wet section of a paper machine) Information provided by Okulen |