LNP THERMOCOMP 9X10401H compound is based on Polyphenylsulfone (PPSU) containing proprietary fillers. Added features of this grade include: Healthcare, X-Ray Opaque. Features: Healthcare,Safety & Detection (X-Ray and Metal Detection) Information provided by SABIC |